Stress Corrosion Cracking: Theory and Practice Reprint Edition

Stress Corrosion Cracking: Theory and Practice Reprint Edition book cover

Stress Corrosion Cracking: Theory and Practice Reprint Edition

Author(s): V. S. Raja (Editor), Tetsuo Shoji (Series Editor)

  • Publisher: Woodhead Publishing
  • Publication Date: 30 Jun. 2016
  • Edition: Reprint
  • Language: English
  • Print length: 818 pages
  • ISBN-10: 0081016468
  • ISBN-13: 9780081016466

Book Description

The problem of stress corrosion cracking (SCC), which causes sudden failure of metals and other materials subjected to stress in corrosive environment(s), has a significant impact on a number of sectors including the oil and gas industries and nuclear power production. Stress corrosion cracking reviews the fundamentals of the phenomenon as well as examining stress corrosion behaviour in specific materials and particular industries. The book is divided into four parts. Part one covers the mechanisms of SCC and hydrogen embrittlement, while the focus of part two is on methods of testing for SCC in metals. Chapters in part three each review the phenomenon with reference to a specific material, with a variety of metals, alloys and composites discussed, including steels, titanium alloys and polymer composites. In part four, the effect of SCC in various industries is examined, with chapters covering subjects such as aerospace engineering, nuclear reactors, utilities and pipelines. With its distinguished editors and international team of contributors, Stress corrosion cracking is an essential reference for engineers and designers working with metals, alloys and polymers, and will be an invaluable tool for any industries in which metallic components are exposed to tension, corrosive environments at ambient and high temperatures.

Editorial Reviews

About the Author

Prof. V.S Raja received his doctorate from the Indian Institute of Science in Bangalore in 1987, then joined the faculty at the Indian Institute of Technology in Bombay, where he is now the Institute Chair Professor in the Department of Metallurgical Engineering and Materials Science. His research focuses broadly on the field of corrosion. He worked as a guest researcher at Chalmers University of Technology in Sweden, as a Visiting Professor at the University of Nevada in the United States, and as a Guest Scientist at GKSS in Germany and Tohoku University in Japan. He is currently working on numerous corrosion-related challenges in Canada, France, Australia, Belgium, and the Netherlands.

He is a member of the CSIR and DRDO laboratories’ Research Councils, and he sat on the NACE international research committee from 2009 to 2013. He has garnered multiple national accolades and is a NACE fellow as a result of his efforts.

Tetsuo Shoji is Professor at the Fracture and Reliability Research Institute at Tohoku University, Japan.

View on Amazon

电子书代发PDF格式价格30元我要求助
未经允许不得转载:Wow! eBook » Stress Corrosion Cracking: Theory and Practice Reprint Edition